PBN flow mark problem in film processing

Problem Phenomenon
Polybutylene naphthalate PBN shows flow mark in film processing at 270-300°C.
Cause Analysis
Oxidation under high-temperature processing at 270-300°C triggers the problem.
Solution
Solved by nitrogen protection.
Key Takeaway
PBN ultra-high-temperature processing requires comprehensive protection.
PBNflow markhigh temperaturefilmprotection