Molding Process
5 views
EPDM under-vulcanization
Problem Phenomenon
Insufficient elasticity and low strength after vulcanization
Cause Analysis
Insufficient vulcanizing agent, insufficient vulcanization temperature and time
Solution
Sulfur 1-2 parts or peroxide at 160-180C
Key Takeaway
Vulcanization is the core of EPDM processing
Was this helpful?
0 people found this helpful