Molding Process
5 views
POE toughened PP chemical resistance drops
Problem Phenomenon
POE toughened PP gasoline immersion swelling >5%
Cause Analysis
POE elastomer high affinity to hydrocarbon solvents, polyolefin nature
Solution
1) POE reduced to 5-8wt%; 2) DCP slight crosslinking to reduce swelling; 3) POE-g-MAH to reduce continuous phase
Key Takeaway
Chemical resistance drop is caused by polyolefin solvent affinity
Was this helpful?
0 people found this helpful