Injection Molding 2 views

TPU '2079851475616104452 cycle too long affecting efficiency

Problem Phenomenon
The '2079851475616104452 cycle exceeds the target by more than 20%
Cause Analysis
Cooling time accounts for a large proportion, plasticization is insufficient, mold opening and closing is slow
Solution
Optimize the cooling water channels, increase the plasticizing capacity, increase mold opening and closing
Key Takeaway
Cycle optimization is the key to increasing production and reducing costs