Molding Process 5 views

Processing temperature too low, poor plasticization

Problem Phenomenon
Below 190C plasticization is insufficient, the surface is rough
Cause Analysis
The temperature is low, not fully melted, plasticization is insufficient
Solution
Raise to the reasonable range of 190-230C
Key Takeaway
The processing temperature window determines plasticization