Molding Process 5 views

Processing temperature too high, EPDM degradation

Problem Phenomenon
The product surface is rough, burnt smell
Cause Analysis
>230C thermal degradation of the EPDM phase
Solution
Strictly control the upper temperature limit
Key Takeaway
The EPDM phase is heat sensitive