Fenómeno do problema
Visible wavy flow marks on the PC product surface, obvious on high-gloss surfaces.
Análise das causas
Front temperature drops too fast or injection speed fluctuates; low mold temperature and a small gate cause unstable filling.
Solução
①Increase mold temperature and melt temperature; ②Optimize the speed curve to keep the front stable; ③Enlarge the gate; ④Check hot runner temperature uniformity.
Conclusão principal
Flow mark treatment = constant front temperature and speed.