Molding Process
4 visualizações
PMMA Sink Marks
Fenómeno do problema
Depressions on the back of thick walls and ribs, appearing as optical distortion in transparent parts.
Análise das causas
Uneven wall thickness + insufficient feeding; hard pressure feeding in turn increases internal stress and induces delayed cracking.
Solução
①Uniform wall thickness (0.635~3.81mm); ②Rib thickness ≤50%~60%; ③Moderate holding pressure; ④Reduce material in thick walls.
Conclusão principal
PMMA sink marks rely on structure, hard pressure trades for delayed cracking.
Isto foi útil?
0 pessoas acharam isto útil