PMMA Sink Marks
Fenómeno del problema
Depressions on the back of thick walls and ribs, appearing as optical distortion in transparent parts.
Análisis de la causa
Uneven wall thickness + insufficient feeding; hard pressure feeding in turn increases internal stress and induces delayed cracking.
Solución
①Uniform wall thickness (0.635~3.81mm); ②Rib thickness ≤50%~60%; ③Moderate holding pressure; ④Reduce material in thick walls.
Conclusión clave
PMMA sink marks rely on structure, hard pressure trades for delayed cracking.