Extrusion & Post 13 visualizações

Material overflow at PU vacuum section

Fenómeno do problema
Material overflows at the vacuum section in PU extrusion, vent hole clogged
Análise das causas
PU melt viscosity low, overflowing at vacuum section; vacuum section temperature too high, viscosity even lower, aggravating overflow; vent hole design improper
Solução
1) Lower vacuum section temperature by 5-10°C to increase viscosity; 2) Add baffle above the vent hole to prevent overflow; 3) Increase screw speed to accelerate conveying and reduce residence
Conclusão principal
Overflow is caused by low melt viscosity; temperature reduction and baffle are key
PU vacuum section overflow melt viscosity temperature reduction vent baffle