Extrusion & Post 13 visualizações

Poor printing adhesion of PVA film

Fenómeno do problema
After printing on PVA film, ink adhesion
Análise das causas
PVA surface polarity has poor affinity with ink; corona treatment effect decays quickly; ink system does not match PVA
Solução
1) Print immediately after corona treatment within 24h; 2) Use PVA-specific ink; 3) Increase corona power to 15-20kW/m² to ensure surface tension >42mN/m; 4) Flame treatment to assist surface polarization
Conclusão principal
Poor printing adhesion is caused by insufficient surface polarity; corona treatment and dedicated ink are the key
PVA filmprinting adhesioncorona treatmentdedicated inksurface tension