Extrusion & Post
14 visualizaciones
Poor printing adhesion of PVA film
Fenómeno del problema
After printing on PVA film, ink adhesion
Análisis de la causa
PVA surface polarity has poor affinity with ink; corona treatment effect decays quickly; ink system does not match PVA
Solución
1) Print immediately after corona treatment within 24h; 2) Use PVA-specific ink; 3) Increase corona power to 15-20kW/m² to ensure surface tension >42mN/m; 4) Flame treatment to assist surface polarization
Conclusión clave
Poor printing adhesion is caused by insufficient surface polarity; corona treatment and dedicated ink are the key