Extrusion & Post 13 visualizações

POE extruder screw severe wear

Fenómeno do problema
After 200h of POE extrusion, screw and barrel wear reaches 0.5mm
Análise das causas
Filler causes large wear to the screw; screw material hardness insufficient, not nitrided; processing temperature too high causes POE to adhere to the screw, aggravating wear
Solução
1) Use nitrided screw or bimetallic screw SK-2 alloy; 2) Lower processing temperature to reduce adhesive wear; 3) Treat filler with coupling agent to reduce friction; 4) Regularly check wear, replace promptly when >0.3mm
Conclusão principal
Screw wear is caused by filler friction and adhesion; wear-resistant screw and temperature control are key
POE extrusionscrew wearnitrided screwfiller frictionbimetallic screw