POE internal stress concentration severe

Fenómeno do problema
POE product internal stress >15MPa causing cracking during storage
Análise das causas
Injection speed too fast, orientation stress large; uneven cooling freezes thermal stress; improper gate position concentrates flow orientation
Solução
1) Reduce injection speed to reduce orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal 80°C/4h to release stress; 4) Optimize gate position
Conclusão principal
Internal stress is caused by fast injection and uneven cooling; reducing speed, uniform cooling and annealing are key
POEinternal stressorientation stressannealing treatmentuniform cooling