Injection Molding 4 views

POE internal stress concentration severe

Problem Phenomenon
POE product internal stress >15MPa causing cracking during storage
Cause Analysis
Injection speed too fast, orientation stress large; uneven cooling freezes thermal stress; improper gate position concentrates flow orientation
Solution
1) Reduce injection speed to reduce orientation; 2) Uniform mold temperature to reduce thermal stress; 3) Anneal 80°C/4h to release stress; 4) Optimize gate position
Key Takeaway
Internal stress is caused by fast injection and uneven cooling; reducing speed, uniform cooling and annealing are key
POEinternal stressorientation stressannealing treatmentuniform cooling