Q
Poor interfacial bonding between EVA and filler
A
Elastomer-filler interface needs dual action of coupling agent and compatibilizer, otherwise filler has negative effect
Material Analysis EVA filler interfacial bonding coupling agent compatibilizer filler dispersion
Q
EVA extrusion melt fracture
A
Melt fracture is caused by elastic recovery exceeding critical value; reducing speed and lengthening die are the core countermeasures
Extrusion & Post EVA extrusion melt fracture elastic recovery die L/D extrusion rate
Q
Bubbles in EVA injection molded thick walls
A
Thick wall bubbles are caused by insufficient holding pressure, moisture and poor venting combined
Material Drying EVA injection bubbles holding pressure thick wall products mold venting
Q
Difficult demolding of EVA '2079851475616104452
A
Difficult demolding is caused by adhesion and insufficient mold design; increasing demolding draft is the fundamental measure
Injection Molding EVA injection difficult demolding demolding draft adhesion ejection design
Q
EMA product elliptical deformation
A
Elliptical deformation is caused by asymmetric demolding force; uniform ejection is key
Molds & Tooling EMA elliptical deformation symmetric ejection uniform cooling setting time
Q
EMA internal delamination cracking
A
Internal delamination is caused by poor interface and shrinkage differences; compatibilizer and uniform cooling are key
Extrusion & Post EMA internal delamination interfacial bonding compatibilizer uniform cooling
Q
EMA surface snakeskin texture
A
Snakeskin texture is caused by low temperature extrusion and elastic recovery; raising temperature and reducing speed are key
Extrusion & Post EMA snakeskin texture extrusion temperature elastic recovery die temperature control
Q
EMA internal black specks carbonization
A
Black specks are caused by thermal carbonization and carbon deposit; lowering temperature and regular cleaning are key
Processing Machinery EMA internal black specks thermal carbonization screw cleaning temperature control
Q
EMA product twist deformation
A
Twist deformation is caused by asymmetric cooling; symmetric cooling is key
Molds & Tooling EMA twist deformation symmetric cooling gate arrangement annealing
Q
Low EMA flexural modulus
A
Low flexural modulus is caused by material softness and insufficient filler; adding rigid filler is key
Material Analysis EMA flexural modulus rigid filler nucleating agent crystallinity