Extrusion & Post 11 görüntüleme

EEA Vacuum Section Material Overflow

Sorun Belirtisi
Material overflows at the vacuum vent section during EEA extrusion, vent hole blocked
Neden Analizi
EEA melt viscosity is low and overflows at the vacuum section; vacuum section temperature is high, viscosity even lower, aggravating overflow; improper vent hole design
Çözüm
1) Lower the vacuum section temperature by 5-10°C to increase viscosity; 2) Add a baffle above the vent hole to prevent overflow; 3) Increase screw speed to accelerate conveying and reduce residence
Temel Çıkarım
Overflow is caused by low melt viscosity; lowering temperature and adding a baffle are key
EEA vacuum section overflow melt viscosity temperature reduction vent baffle