Extrusion & Post 14 visualizaciones

EEA Vacuum Section Material Overflow

Fenómeno del problema
Material overflows at the vacuum vent section during EEA extrusion, vent hole blocked
Análisis de la causa
EEA melt viscosity is low and overflows at the vacuum section; vacuum section temperature is high, viscosity even lower, aggravating overflow; improper vent hole design
Solución
1) Lower the vacuum section temperature by 5-10°C to increase viscosity; 2) Add a baffle above the vent hole to prevent overflow; 3) Increase screw speed to accelerate conveying and reduce residence
Conclusión clave
Overflow is caused by low melt viscosity; lowering temperature and adding a baffle are key