Molds & Tooling 5 görüntüleme

Internal shrinkage voids of PU

Sorun Belirtisi
Shrinkage voids of 0.5-2mm diameter in the center of PU thick-walled products
Neden Analizi
After cooling of thick-walled area, interior shrinks but surface already solidified, cannot be fed; holding time insufficient, gate freezes too early
Çözüm
1) Extend holding time until the gate is completely frozen; 2) Increase gate size to delay freezing; 3) Product design to reduce wall thickness differences
Temel Çıkarım
Shrinkage voids are caused by thick-wall shrinkage and insufficient holding; extending holding is key
PU shrinkage void thick wall holding time gate freezing

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu