Molds & Tooling 8 visualizaciones

Internal shrinkage voids of PU

Fenómeno del problema
Shrinkage voids of 0.5-2mm diameter in the center of PU thick-walled products
Análisis de la causa
After cooling of thick-walled area, interior shrinks but surface already solidified, cannot be fed; holding time insufficient, gate freezes too early
Solución
1) Extend holding time until the gate is completely frozen; 2) Increase gate size to delay freezing; 3) Product design to reduce wall thickness differences
Conclusión clave
Shrinkage voids are caused by thick-wall shrinkage and insufficient holding; extending holding is key
PU shrinkage void thick wall holding time gate freezing