Material Analysis 8 görüntüleme

Fiber content inspection inaccurate

Sorun Belirtisi
The fiber content measured by the ashing method fluctuates from the formulation value by >3%
Neden Analizi
PP does not pyrolyze completely during ashing, leaving carbides causing high mass; the glass fiber itself loses mass during high-temperature ashing (>600°C); sampling representativeness is insufficient
Çözüm
Standardize ashing conditions (constant temperature at 550°C for 2 hours); use TGA (thermogravimetric analysis) to accurately measure each component; take samples at multiple points and mix to improve representativeness
Temel Çıkarım
Fiber content is the core indicator of LGFPP quality inspection, and the inspection method needs to be standardized
fiber contentashing methodTGAsampling representativenessquality inspection