Material Analysis
10 visualizações
Fiber content inspection inaccurate
Fenómeno do problema
The fiber content measured by the ashing method fluctuates from the formulation value by >3%
Análise das causas
PP does not pyrolyze completely during ashing, leaving carbides causing high mass; the glass fiber itself loses mass during high-temperature ashing (>600°C); sampling representativeness is insufficient
Solução
Standardize ashing conditions (constant temperature at 550°C for 2 hours); use TGA (thermogravimetric analysis) to accurately measure each component; take samples at multiple points and mix to improve representativeness
Conclusão principal
Fiber content is the core indicator of LGFPP quality inspection, and the inspection method needs to be standardized
Isto foi útil?
0 pessoas acharam isto útil