Material Drying
6 مشاهدة
Control of strength abnormality in PEOX calendering packaging
ظاهرة المشكلة
During PEOX calendering production of packaging, the problem of uneven strength occurs.
تحليل الأسباب
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.1% exceeding the standard, and excessively long residence time.
الحل
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
الخلاصة الأساسية
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.