Material Drying
7 visualizações
Control of strength abnormality in PEOX calendering packaging
Fenómeno do problema
During PEOX calendering production of packaging, the problem of uneven strength occurs.
Análise das causas
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.1% exceeding the standard, and excessively long residence time.
Solução
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Conclusão principal
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
Isto foi útil?
0 pessoas acharam isto útil
Obrigado pelo seu comentário!