Material Drying
8 visualizaciones
Control of strength abnormality in PEOX calendering packaging
Fenómeno del problema
During PEOX calendering production of packaging, the problem of uneven strength occurs.
Análisis de la causa
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.1% exceeding the standard, and excessively long residence time.
Solución
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Conclusión clave
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.
¿Le ha resultado útil?
0 personas encontraron esto útil