Control of strength abnormality in PEOX calendering packaging
Problembeschreibung
During PEOX calendering production of packaging, the problem of uneven strength occurs.
Ursachenanalyse
Mainly due to the processing temperature deviating from the window +65-95°C, moisture content >0.1% exceeding the standard, and excessively long residence time.
Lösung
Strictly control the temperature within the recommended range, fully dry the material to moisture content <0.1%, and reduce the screw speed.
Wichtigste Erkenntnis
PEOX processing requires precise control of the three elements of temperature, humidity, and residence time.