Extrusion & Post 2 Aufrufe

LDPE '2079851475616104452 Mold Sticking

Problembeschreibung
Soft LDPE parts are strained and deformed during demolding.
Ursachenanalyse
LDPE is soft and easily stretched and deformed during ejection; small draft angle and poor cavity polishing aggravate it.
Lösung
①Increase draft angle; ②polish the cavity; ③reduce holding pressure; ④extend cooling to improve rigidity; ⑤enlarge ejection area.
Wichtigste Erkenntnis
Soft material demolding = draft angle + polishing + ejection area.
LDPE; '2079851475616104452; mold sticking; draft angle; ejection