Extrusion & Post 3 visualizaciones

LDPE '2079851475616104452 Mold Sticking

Fenómeno del problema
Soft LDPE parts are strained and deformed during demolding.
Análisis de la causa
LDPE is soft and easily stretched and deformed during ejection; small draft angle and poor cavity polishing aggravate it.
Solución
①Increase draft angle; ②polish the cavity; ③reduce holding pressure; ④extend cooling to improve rigidity; ⑤enlarge ejection area.
Conclusión clave
Soft material demolding = draft angle + polishing + ejection area.