Extrusion & Post
7 visualizações
LDPE '2079851475616104452 Mold Sticking
Fenómeno do problema
Soft LDPE parts are strained and deformed during demolding.
Análise das causas
LDPE is soft and easily stretched and deformed during ejection; small draft angle and poor cavity polishing aggravate it.
Solução
①Increase draft angle; ②polish the cavity; ③reduce holding pressure; ④extend cooling to improve rigidity; ⑤enlarge ejection area.
Conclusão principal
Soft material demolding = draft angle + polishing + ejection area.