MP insufficient flatness
Problembeschreibung
MP flat products flatness >0.5mm/100mm, warpage
Ursachenanalyse
MP shrinkage large and anisotropic; mold cooling uneven; residual stress release causing continuous warpage
Lösung
1) uniform mold temperature to reduce temperature difference; 2) increase holding pressure to reduce shrinkage difference; 3) annealing to release residual stress
Wichtigste Erkenntnis
insufficient flatness is caused by shrinkage difference and stress; uniform cooling and annealing are key