Molds & Tooling 5 görüntüleme

MP insufficient flatness

Sorun Belirtisi
MP flat products flatness >0.5mm/100mm, warpage
Neden Analizi
MP shrinkage large and anisotropic; mold cooling uneven; residual stress release causing continuous warpage
Çözüm
1) uniform mold temperature to reduce temperature difference; 2) increase holding pressure to reduce shrinkage difference; 3) annealing to release residual stress
Temel Çıkarım
insufficient flatness is caused by shrinkage difference and stress; uniform cooling and annealing are key
MP flatness shrinkage difference uniform mold temperature annealing