Molds & Tooling 8 visualizaciones

MP insufficient flatness

Fenómeno del problema
MP flat products flatness >0.5mm/100mm, warpage
Análisis de la causa
MP shrinkage large and anisotropic; mold cooling uneven; residual stress release causing continuous warpage
Solución
1) uniform mold temperature to reduce temperature difference; 2) increase holding pressure to reduce shrinkage difference; 3) annealing to release residual stress
Conclusión clave
insufficient flatness is caused by shrinkage difference and stress; uniform cooling and annealing are key
MP flatness shrinkage difference uniform mold temperature annealing