Low burst pressure of PET extruded pipes

Problembeschreibung
The burst pressure of PET extruded pipes in pressure testing is lower than design requirements.
Ursachenanalyse
Pipe wall thickness is uneven or has weak points; weld lines (die head spider marks) have insufficient strength; material IV is on the low side; haul-off over-stretches.
Lösung
Optimize the die head to reduce weld lines; control wall thickness uniformity; select high-IV raw materials (≥0.80); optimize haul-off speed.
Wichtigste Erkenntnis
PET pipe burst strength depends on wall thickness uniformity and material intrinsic viscosity.
PETpipeburst pressurewall thicknessweld line