Injection Molding
3 Aufrufe
PETG '2079851475616104452 low production efficiency, long cycle
Problembeschreibung
The molding cycle is too long, cooling time accounts for a large proportion, and capacity is insufficient.
Ursachenanalyse
Cooling time too long, melt temperature high requiring longer cooling, mold cooling efficiency insufficient.
Lösung
Lower the melt temperature to 220-240°C; optimize the mold cooling water channels to improve efficiency; use a low-temperature mold temperature controller.
Wichtigste Erkenntnis
PETG molding cycle optimization mainly starts from cooling efficiency.