PETG '2079851475616104452 low production efficiency, long cycle
Fenómeno do problema
The molding cycle is too long, cooling time accounts for a large proportion, and capacity is insufficient.
Análise das causas
Cooling time too long, melt temperature high requiring longer cooling, mold cooling efficiency insufficient.
Solução
Lower the melt temperature to 220-240°C; optimize the mold cooling water channels to improve efficiency; use a low-temperature mold temperature controller.
Conclusão principal
PETG molding cycle optimization mainly starts from cooling efficiency.