Injection Molding 8 görüntüleme

PETG '2079851475616104452 low production efficiency, long cycle

Sorun Belirtisi
The molding cycle is too long, cooling time accounts for a large proportion, and capacity is insufficient.
Neden Analizi
Cooling time too long, melt temperature high requiring longer cooling, mold cooling efficiency insufficient.
Çözüm
Lower the melt temperature to 220-240°C; optimize the mold cooling water channels to improve efficiency; use a low-temperature mold temperature controller.
Temel Çıkarım
PETG molding cycle optimization mainly starts from cooling efficiency.
PETGmolding cyclecooling efficiencymelt temperature

Bu faydalı oldu mu?

0 kişi bunu faydalı buldu

ChemAI