Extrusion & Post 2 visualizaciones

PCABS FDM printing temperature

Fenómeno del problema
【Problem Phenomenon】PC/ABS filament printing has weak interlayer or deformation, improper parameters
Análisis de la causa
PC/ABS FDM nozzle 250-270℃, bed temperature 100-110℃, requires an enclosed chamber; higher temperature than pure ABS, interlayer strength depends on full melting
Solución
Nozzle 250-270℃, bed temperature 100-110℃; enclosed chamber; filament dried at 60-80℃ for 4h; after adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PC/ABS printing 250-270℃ with an enclosed chamber; after confirming effectiveness, fix the parameters and practices into the work instruction to prevent recurrence; include this case in the defect archive as a troubleshooting reference for similar problems later
FDMprinting temperaturebed temperaturechamber