PC extrusion sheet temperature

Fenómeno del problema
【Problem Phenomenon】PC extruded sheet has bubbles or poor surface, improper temperature
Análisis de la causa
PC extrusion melt temperature 250-290℃, slightly lower than '2079851475616104452; raw material must be fully dried; die temperature affects the surface;During on-site troubleshooting, verify item by item according to this mechanism, and avoid blindly adjusting the machine based solely on experience
Solución
Dry at 120℃×3-4h before extrusion; melt temperature 250-290℃; die temperature matched;After adjustment, take continuous samples to verify the effect, and resume mass production only after confirming stability
Conclusión clave
PC extrusion dries first, melt temperature 250-290℃;After confirming effectiveness, solidify the parameters and practices into the work instruction to prevent recurrence;Include this case in the defect archive as a reference for troubleshooting similar problems in the future