Molds & Tooling 8 visualizaciones

Correlation between silver streaks on the surface of PETG products and gate position

Fenómeno del problema
Silver streaks are concentrated near the gate and spread toward the middle of the product.
Análisis de la causa
The shear heat at the gate is the highest and the water vaporizes most violently, and shear-induced degradation occurs in the gate area.
Solución
Appropriately reduce the injection speed in the gate area; fully dry; optimize the gate size.
Conclusión clave
PETG gate area silver streaks point to shear and moisture.