Injection Molding 3 views

DSTDP surface orange peel texture

Problem Phenomenon
DSTDP product surface orange-peel-like uneven texture, rough hand feel
Cause Analysis
Mold temperature on the low side <30°C, product surface rapidly cools and solidifies, then the interior continues to shrink causing surface unevenness; injection speed too low
Solution
1) Raise mold temperature to 40-50°C to delay surface solidification; 2) appropriately increase injection speed; 3) increase holding pressure to reduce internal shrinkage
Key Takeaway
Orange peel texture is caused by rapid cooling and solidification; raising mold temperature and holding pressure are key