Injection Molding 2 views

Insufficient filling of PLA '2079851475616104452 (short shot)

Problem Phenomenon
The cavity is not completely filled during PLA '2079851475616104452.
Cause Analysis
The PLA melt viscosity is relatively large and the fluidity is not as good as PP, etc.; the injection pressure and speed are insufficient; the melt temperature is low; the gate is too small.
Solution
Raise the melt temperature to 180-200°C; increase the injection pressure and speed; enlarge the gate; the mold temperature can be appropriately lowered.
Key Takeaway
PLA fluidity is the main cause of short shots.