Injection Molding 14 visualizações

HDPE injection molded product sink marks - thick-walled type

Fenómeno do problema
Thick-walled HDPE parts have severe surface depressions.
Análise das causas
Excessive wall thickness means large shrinkage, which conventional holding pressure cannot compensate; PP/PE thick-walled parts should be structurally material-reduced.
Solução
①Core out thick walls to reduce material; ②gate near the thick wall; ③increase holding pressure; ④strengthen cooling.
Conclusão principal
For thick-wall sink marks, structural material reduction is prioritized.
HDPE; '2079851475616104452; sink mark; thick wall; material reduction