Molds & Tooling 7 visualizações

EVA flatness is insufficient

Fenómeno do problema
EVA flat product flatness >0.5mm/100mm warpage
Análise das causas
EVA shrinkage rate is large and differs in all directions; uneven mold cooling; residual stress release causing continuous warpage
Solução
1) Uniform mold temperature to reduce temperature differences; 2) Increase holding pressure to reduce shrinkage differences; 3) Annealing to release residual stress
Conclusão principal
Insufficient flatness is caused by shrinkage differences and stress; uniform cooling and annealing are key