Extrusion & Post 5 visualizações

Stringing problem in PETG 3D printing

Fenómeno do problema
During PETG FDM 3D printing, stringing and hair-like thin filaments are produced when the nozzle moves.
Análise das causas
Printing temperature is on the high side; melt viscosity is too low and thin filaments are drawn out; retraction parameters are set improperly, with insufficient retraction distance or speed.
Solução
Reduce printing temperature to 220-235°C; increase retraction distance to 4-6mm and speed to 30-50mm/s; enable the wipe function.
Conclusão principal
PETG 3D printing stringing is solved by lowering temperature and optimizing retraction parameters.
PETG3D printingstringingprinting temperatureretraction

Isto foi útil?

0 pessoas acharam isto útil

ChemAI