Injection Molding 12 görüntüleme

HDPE injection molded product melt temperature unevenness

Sorun Belirtisi
Some areas of the same-mold products have inconsistent gloss and shrinkage.
Neden Analizi
Uneven plasticization and large melt temperature difference; insufficient back pressure or poor screw mixing ability.
Çözüm
①Increase back pressure; ②check the screw mixing section; ③stabilize the melt temperature curve; ④replace with a mixing-type screw if necessary.
Temel Çıkarım
Melt uniformity relies on back pressure and screw mixing.
HDPE; '2079851475616104452; melt unevenness; back pressure; mixing