Extrusion & Post 3 visualizaciones

LDPE Extrusion Coating Neck-in

Fenómeno del problema
During extrusion coating/lamination, the two edges of the molten film shrink back, and the effective coating width narrows.
Análisis de la causa
Elastic shrinkage of the molten film after exiting the die + fast edge cooling; low die temperature, fast haul-off and large melt elasticity all increase neck-in.
Solución
①Raise melt temperature; ②reduce haul-off speed; ③optimize air gap distance; ④select low neck-in grades.
Conclusión clave
Neck-in = elastic shrinkage; adjust oppositely to lowering temperature and increasing speed.